| NORM | TITLE | 
|---|---|
| ISO 11357 | Plastics - Differential scanning calorimetry (DSC) - Part 1: General principles (ISO 11357-1:2016) | 
| ISO 11357 | Plastics - Differential scanning calorimetry (DSC) - Part 1: General principles (ISO 11357-1:2016) | 
| ISO 11409 | Plastics - Phenolic resins - Determination of heat and reaction temperatures by differential scanning calorimetry (ISO 11409:1993); German version EN ISO 11409:1998 | 
| ISO 10837 | Determination of the thermal stability of polyethylene (PE) for use in gas pipes and fittings | 
| DIN EN 728 | Plastics piping and ducting systems - Polyolefin pipes and fittings - Determination of oxidation induction time | 
| DIN 65467 | Aerospace - Testing of thermoset resin systems with and without reinforcement - DSC method | 
| ASTM E 794 | Standard test methods for melting and crystallization temperatures by thermal analysis | 
| ASTM D 4565 | Standard test methods for physical and environmental performance characteristics of insulation and sheathing for telecommunication wires and cables | 
| ASTM D 3895 | Standard test method for oxidation induction time of polyolefins by differential scanning calorimetry | 
| ASTM C 351 | Standard Test Method for Mean Specific Heat of Thermal Insulation | 
| ASTM E967 | Standard Test Method for Temperature Calibration of Differential Scanning Calorimeters and Differential Thermal Analyzers | 
| ASTM E968 | Standard Practice for Heat Flow Calibration of Differential Scanning Calorimeters | 
| ASTM E793 | Standard Test Method for Enthalpies of Fusion and Crystallization by Differential Scanning Calorimetry | 
| ASTM D3895 | Standard Test Method for Oxidative-Induction Time of Polyolefins by Differential Scanning Calorimetry | 
| ASTM D3417 | Standard Test Method for Enthalpies of Fusion and Crystallization of Polymers by Differential Scanning Calorimetry (DSC) (Withdrawn 2004) | 
| ASTM D3418 | Standard Test Method for Enthalpies of Fusion and Crystallization of Polymers by Differential Scanning Calorimetry (DSC) (Withdrawn 2004) | 
| ASTM E1269 | Standard Test Method for Determining Specific Heat Capacity by Differential Scanning Calorimetry | 
| DIN 51004 | Thermal analysis (TA); determination of the melting temperatures of crystalline materials using differential thermal analysis (DTA) | 
| DIN 51007 | Thermal Analysis (TA) - Differential Thermal Analysis (DTA) and Differential Scanning Calorimetry (DSC) - General Basics | 
| DIN 53765 | Testing of plastics and elastomers; thermal analysis; differential scanning calorimetry (DSC) | 
Normas para analizadores termogravimétricos
| NORM | TITLE | 
|---|---|
| ISO 11358 | Plastics - Thermogravimetry (TG) of polymers - Part 1: General principles (ISO 11358-1:2014) | 
| ISO 11358 | Plastics - Thermogravimetry (TG) of polymers - Part 1: General principles (ISO 11358-1:2014) | 
| ISO 7111 | Plastics - Thermogravimetry of polymers - Temperature scanning method | 
| DIN 51006 | Thermal analysis (TA) - Thermogravimetry (TG) - Fundamentals | 
| ASTM E 914 | Practice for the evaluation of the temperature scale for thermogravimetry (withdrawn 1994) | 
| ASTM E 1868 | Standard test methods for loss drying by thermogravimetry | 
| ASTM D 3175 | Standard test methods for volatile substances in the analytical sample of coal and coke | 
| ISO/DIS 9924 | Rubber and rubber products - Determination of the composition of vulcanizates and uncured compounds by thermogravimetry - Part 1: Butadiene, ethylene-propylene copolymer and terpolymer, isobutene-isoprene, isoprene and styrene-butadiene rubbers | 
| ASTM E1131 | Standard Test Method for Compositional Analysis by Thermogravimetry | 
| ASTM D3850 | Standard Test Method for Rapid Thermal Degradation of Solid Electrical Insulating Materials By Thermogravimetric Method (TGA) | 
| ASTM D6375 | Standard Test Method for Evaporation Loss of Lubricating Oils by Thermogravimetric Analyzer (TGA) Noack Method | 
| ASTM D6370 | Standard Test Method for Rubber—Compositional Analysis by Thermogravimetry (TGA) | 
| ASTM E2550 | Standard Test Method for Thermal Stability by Thermogravimetry | 
| ASTM D3175 | Standard Test Method for Volatile Matter in the Analysis Sample of Coal and Coke | 
Normas para analizadores termomecánicos
| NORM | TITLE | 
|---|---|
| DIN 51005 | Thermal analysis (TA) - Terms | 
| DIN 12667 | Thermal performance of building materials and products - Determination of thermal resistance by protected hot plate and heat flow meter methods - High and medium thermal resistance products; German version EN 12667:2001 | 
| ASTM D 3418 | Standard test methods for transition temperatures and enthalpies of fusion and crystallization of polymers by differential scanning calorimetry | 
| ASTM D 3417 | Standard test methods for enthalpies of melting and crystallization of polymers by differential scanning calorimetry (DSC) (withdrawn 2004) | 
| ISO 11359-2 | Plastics - Thermomechanical analysis (TMA) - Part 2: Determination of the coefficient of linear thermal expansion and glass transition temperature | 
| IPC-TM-650 2.4.24 | Glass transition temperature and thermal expansion of the Z-axis using TMA | 
| DIN 51005 | Thermal analysis (TA) - Terms | 
| IPC-TM-650 2.4.41 | Linear coefficient of thermal expansion of electrical insulating materials | 
| IPC-TM-650 2.4.24.1 | Time to delamination (TMA method) | 
| IPC-TM-650 2.4.41.3 | Coefficient of thermal expansion in the plane, OrganicFilms | 
| IPC-TM-650 2.4.24.3 | Glass transition temperature of organic films - TMA method | 
| ENV 1159-3 | Advanced technical ceramics - Ceramic composites, thermophysical properties - Part 3: Determination of specific heat capacity | 
| DIN 53752 | Testing of plastics; determination of the coefficient of linear thermal expansion | 
| DIN 53545 | Testing of rubber - Determination of the low temperature behavior of elastomers - Principles and test methods | 
| CEI/IEC 1006 | Test methods for determining the glass transition temperature of electrical insulating materials | 
| ASTM E 2347 | Standard test method for indentation softening temperature by thermomechanical analysis | 
| ASTM E 1824 | Standard test method for assigning a glass transition temperature by thermomechanical analysis: Tensile method | 
| ASTM E 2113 | Standard test method for the extension calibration of thermomechanical analyzers | 
| ASTM E 2092 | Standard test method for the deformation temperature at three-point bending by thermomechanical analysis | 
| ASTM E 1545 | Standard test method for the determination of the glass transition temperature by thermomechanical analysis | 
| ASTM D 3386 | Standard Test Method for Linear Thermal Expansion Coefficient of Electrical Insulating Materials1 | 
| ASTM E831 | Standard Test Method for Linear Thermal Expansion of Solid Materials by Thermomechanical Analysis | 
| ASTM D696 | Standard Test Method for Coefficient of Linear Thermal Expansion of Plastics Between −30°C and 30°C with a Vitreous Silica Dilatometer | 
| ISO 11359 – Parts 1 to 3 | Plastics — Thermomechanical analysis (TMA) — Part 3: Determination of penetration temperature | 
| DIN 51045 | Determination of thermal expansion of solids - Part 1: Fundamentals | 
Normas para dilatómetros
| NORM | TITLE | 
|---|---|
| ASTM E831 | Standard Test Method for Linear Thermal Expansion of Solid Materials by Thermomechanical Analysis | 
| ASTM A 1033 | Standard method for quantitative measurement and reporting of hypo-eutectoid carbon and low-alloy steel phase transformations | 
| ASTM D696 | Standard Test Method for Coefficient of Linear Thermal Expansion of Plastics Between −30°C and 30°C with a Vitreous Silica Dilatometer | 
| ASTM C372 | Standard Test Method for Linear Thermal Expansion of Porcelain Enamel and Glaze Frits and Fired Ceramic Whiteware Products by the Dilatometer Method | 
| DIN 51045 | Determination of thermal expansion of solids - Part 1: Fundamentals | 
Normas de conductividad térmica
| NORM | TITLE | 
|---|---|
| ASTM E1461 | Standard Test Method for Thermal Diffusivity by the Flash Method | 
| DIN 30905 | Thermophysical properties of hard metals - Measurement of thermal diffusivity using the laser flash (heat pulse) method | 
| JIS A 1412 | Test methods for thermal resistance and related properties of thermal insulation - Heat flux meter | 
| ASTM D 5470 | Standard test method for thermal transmission properties of thermally conductive electrical insulation materials | 
| DIN EN 821 | Advanced technical ceramics – Monolithic ceramics, thermo-physical properties – Part 2: Determination of thermal diffusity by the laser flash (or heat pulse) method | 
| BS EN 1159-2 | Advanced technical ceramics. Ceramic composites. Thermophysical properties. Determination of thermal diffusivity | 
| ASTM C714 | Standard Test Method for Thermal Diffusivity of Carbon and Graphite by Thermal Pulse Method | 
| ASTM C518 | Standard Test Method for Steady-State Thermal Transmission Properties by Means of the Heat Flow Meter Apparatus | 
| ISO 8301 | Thermal Insulation; Determination of Steady-State Thermal Transmission Resistance and Related Properties; Method Using the Heat Flow Meter Apparatus | 
| DIN EN 12667 EN 12 | Thermal performance of building materials and products - Determination of thermal resistance by the plate apparatus and heat flow meter apparatus - High and medium thermal resistance products; German version EN 12667:2001 | 
Atención al cliente
Nuestro servicio ofrece
Elige entre las siguientes áreas:
 
															Servicio y reparación
Te ofrecemos varios servicios: Mantenimiento, reparaciones, formación y mucho más.
 
															Asistencia remota
¿Ayuda rápida y competente a través de Teamviewer? Puedes encontrar instrucciones detalladas aquí
 
															Aplicaciones
En la biblioteca de aplicaciones encontrarás algunas publicaciones con nuestros aparatos de medición
 
															Seminarios web a la carta
Haz clic aquí para ver un resumen de nuestros seminarios a la carta. Regístrate y ¡empieza!
 
															Apoyo universitario
Apoyamos a las universidades y escuelas superiores en la adquisición de nuevos aparatos de medición
Ayuda a través de
Servicio-Hotline
Servicio Linseis-Línea Directa
Si necesitas ayuda con problemas técnicos o tienes preguntas sobre el uso del aparato, siempre recibirás una respuesta rápida de nuestro servicio de atención telefónica.
Nuestro servicio está disponible de lunes a jueves de 8 a 16 h y los viernes de 8 a 12 h.
También puedes escribirnos utilizando el formulario de contacto.
Te responderemos en el plazo de un día laborable. 
Así podremos ayudarte lo antes posible:
- Ten a mano el número de serie del aparato averiado (cerca del enchufe, en la placa de características).
- Indícanos dónde se encuentra el aparato (ciudad y país)
- Indícanos tus datos de contacto donde podamos localizarte directamente (correo electrónico y número de teléfono)